This standard specifies a method of evaluation of the susceptibility to hydrogen induced cracking (HIC) of steel products with nominal thicknesses equal to or greater than 6 mm. Note: This standard may be applied by agreement to products with nominal thicknesses lower than 6 mm. This standard does not cover resistance to other types of corrosion such as for example stress corrosion cracking.